AEGIS OGS touch panel
- Truly Semiconductors
- Aug 3, 2022
- 1 min read

By laser and chemical cutting and strength glue coating during production, the damage to the edge of the OGS glass is reduced and the strength is enhanced. High strength and shock resistance of up to 700 MPa is achieved.